The Journal of the American Dental Association
HOME HELP FEEDBACK SUBSCRIPTIONS ARCHIVE SEARCH TABLE OF CONTENTS
 QUICK SEARCH:   [advanced]


     


J Am Dent Assoc, Vol 138, No 3, 349-354.
© 2007 American Dental Association

This Article
Right arrow Abstract Freely available
Right arrow Full Text (PDF)
Right arrow Alert me when this article is cited
Right arrow Alert me if a correction is posted
Services
Right arrow Similar articles in this journal
Right arrow Similar articles in PubMed
Right arrow Alert me to new issues of the journal
Right arrow Download to citation manager
Right arrow reprints & permissions
Citing Articles
Right arrow Citing Articles via HighWire
Right arrow Citing Articles via Google Scholar
Google Scholar
Right arrow Articles by Feuerstein, O.
Right arrow Articles by Weiss, E. I.
Right arrow Search for Related Content
PubMed
Right arrow PubMed Citation
Right arrow Articles by Feuerstein, O.
Right arrow Articles by Weiss, E. I.
Related Collections
Right arrow Infection Control

RESEARCH

JADA Continuing Education

Antibacterial properties of self-etching dental adhesive systems



Osnat Feuerstein, PhD, DMD, Shlomo Matalon, DMD, Hagay Slutzky, DMD and Ervin I. Weiss, DMD


   ABSTRACT
 TOP
 ABSTRACT
 MATERIALS AND METHODS
 RESULTS
 DISCUSSION
 CONCLUSION
 REFERENCES
 
Background. Dental adhesives with antibacterial properties may reduce recurrent or secondary caries. The authors conducted a study to examine the immediate and long-lasting antibacterial properties of four self-etching adhesive systems.

Methods. The authors used the agar diffusion test (ADT) and direct contact test (DCT) to measure the antibacterial properties of AdheSe (Ivoclar Vivadent, Schaan, Liechtenstein), Adper Prompt L-Pop (3M ESPE, Seefeld, Germany), Clearfil Protect Bond (Kuraray, Kurashiki, Okayama, Japan) and Xeno III (Dentsply, Konstanz, Germany) on Streptoccocus mutans after aging samples in phosphate-buffered saline for one, two, seven and 14 days.

Results. Only Clearfil Protect Bond showed an inhibition halo in the ADT. In the DCT, fresh samples of all of the tested materials exhibited potent antibacterial properties, which were maintained by AdheSe for one day and Clearfil Protect Bond for seven days. None of the adhesive systems exhibited any antibacterial properties after 14 days.

Conclusions. All of the tested adhesives had an immediate bactericidal effect on S. mutans. None, however, had long-lasting antibacterial properties.

Clinical Implications. The application of self-etching adhesive materials could contribute to the immediate elimination of residual bacteria. The likelihood of developing secondary caries as a consequence of bacterial microleakage may not be affected by the use of the adhesive systems tested in this study.

Key Words: Adhesives; dental bonding; bacteria; microleakage; antibacterial

Abbreviations: ADT: Agar diffusion test. • BHI: Brain-heart infusion. • DCT: Direct contact test. • DDW: Double-distilled water. • MDPB: 12-Methacryloyl oxydodecylpyridinium bromide. • OD: Optical density. • PBS: Phosphate-buffered saline.

Self-etching dental adhesive systems have been developed to simplify bonding procedures and to make their application less time-consuming. In two-step systems—the so-called self-priming and self-etching adhesives—the primer and adhesive are combined into one solution. In one-step systems—the so-called all-in-one adhesives—the etchant, primer and adhesive are combined into one solution. Reducing the steps of the adhesive procedure makes it possible to decrease the application time and the risk of error. On the other hand, the bond strengths of the all-in-one adhesives may be lower than those of the two-step systems.1 A 2004 clinical study showed that simplified systems might restrict the efficacy of the bonding.2

Residual bacteria in the oral cavity may remain at the tooth-restoration interface and increase the risk of developing recurrent caries. This is due to the contaminated smear layer, which is partially incorporated into the hybrid layer.3 In vitro studies have shown that the tooth-restoration interface created when using self-etching adhesive systems do not eliminate microleakage and bacterial penetration, which can lead to secondary caries, the most common reason for dental restoration failure.4,5

Therefore, the antibacterial properties of adhesive materials are important.611 The antibacterial effects of nonpolymerized or immediately polymerized adhesives are beneficial in the eradication of residual bacteria in the oral cavity.6 The long-lasting antibacterial activity of polymerized adhesives may be effective in inactivating bacteria that invade the tooth-adhesive interface by microleakage.

Studies have shown the antibacterial effect of adhesive materials is due to their low pH or to specific antibacterial components such as glu-taraldehyde8,11,12 or 12-methacryloyloxydode-cylpyridinium bromide (MDPB).13 Since copolymerization should immobilize MDPB in the adhesive material, adhesives containing MDPB may be effective against bacteria that invade through microleakage.13

We conducted a study to examine the immediate and long-lasting antibacterial effect of polymerized self-etching adhesive systems on Streptoccocus mutans by using the direct contact test (DCT) and comparing these results with those of the agar diffusion test (ADT).


   MATERIALS AND METHODS
 TOP
 ABSTRACT
 MATERIALS AND METHODS
 RESULTS
 DISCUSSION
 CONCLUSION
 REFERENCES
 
Tested materials. We tested the following four commercially available self-etching adhesive systems:

– AdheSe (Ivoclar Vivadent, Schaan, Liechtenstein), a two-step self-etching product;
– Clearfil Protect Bond (Kuraray, Kurashiki, Okayama, Japan), a two-step self-etching product that has adhesives containing MDPB;
– Adper Prompt L-Pop (3M ESPE, Seefeld, Germany), a one-step self-etching product;
– Xeno III (Dentsply, Konstanz, Germany), a one-step self-etching product.

Tested microorganism. We used S. mutans, the primary etiologic agent for caries, to test the antimicrobial activity of restorative materials.1417 S. mutans 27351M (obtained from the Department of Human Microbiology, Sackler School of Medicine, Tel Aviv University, Israel) is naturally resistant to bacitracin. We grew S. mutans aerobically from frozen stock cultures in brain-heart infusion (BHI) that contained 8 micrograms of bacitracin per milliliter for 48 hours at 37 C.

Experimental design. We performed an ADT on a mitis salivarius agar plate, in which we punched eight holes that were 4 millimeters in diameter. We inoculated the plate with 200 microliters of freshly grown S. mutans (optical density [OD] 650 nanometers = 0.5) spread evenly with a Drigalsky glass stick. After mixing each of the four tested materials, we immediately filled the holes (two holes per material) and light-polymerized them using a light-curing unit (VIP, Bisco, Schaumburg, Ill.) according to the manufacturer’s instructions. We incubated the plates for 72 hours at 37 C and then inspected them for the presence of an inhibition zone. We took two perpendicular measurements of the inhibition halo diameter using a digimatic caliper. We repeated the ADT three times.

The DCT described by Weiss and colleagues1822 is based on bacterial growth in a 96-well microtiter plate (96 MicroWell Plates, Nunc, Copenhagen, Denmark) (Figure 1Go). To create samples, we evenly coated the side walls of eight wells with a tested material and polymerized the material using a light-curing unit as follows:


Figure 1
View larger version (30K):
[in this window]
[in a new window]

 
Figure 1. Schematic drawing of direct contact test performed in a 96-well flat-bottomed microtiter plate. Each material was tested eight times. Bacteria were in direct contact with the tested material for one hour. Growth medium was added. The microtiter plate was vortexed for two minutes and inserted into a temperature-controlled spectrophotometer. Bacterial outgrowth was monitored every 30 minutes for at least 16 hours.

 
– for AdheSe, we applied the primer and brushed it for 30 seconds and then applied the bonding agent and light cured it for 20 seconds;
– for Adper Prompt L-Pop, we rubbed on the adhesive for 15 seconds, dried it and light cured it for 10 seconds;
– for Clearfil Protect Bond, we applied the primer for 20 seconds and dried it and then applied the bonding agent and light cured it for 10 seconds;
– for Xeno III, we mixed the primer and bonding agent together, applied the mixture for 20 seconds and light cured it for 10 seconds.

We rinsed all of the tested materials with phosphate-buffered saline (PBS) before inoculating them with bacteria.

We placed 10 µL of the bacterial suspension (the S. mutans and BHI mixture) (106 cells) on the samples. We incubated the plate for one hour at 37 C until the bacterial suspension evaporated to ensure direct contact between the bacteria and the surface of the tested material. We then turned the plate horizontally, added 220 µL of BHI, placed the plate in a vortex at 100 revolutions per minute for two minutes and inserted it into a temperature-controlled spectrophotometer. We recorded the kinetics of the outgrowth in each well (OD at 650 nm) every 30 minutes for at least 16 hours (VersaMax, Molecular Device, Menlo Oaks Center, Menlo Park, Calif.) set to 37 C. We performed calibration experiments simultaneously for each plate to obtain a comparative quantitative scale. We placed bacteria (106 cells) on each side wall of three wells and added 250 µL of BHI. We performed consecutive fivefold dilution transfers into six sets of three wells. We plotted the average OD measured in three wells simultaneously on a growth curve. In the DCT, each plate was an independent experiment containing positive and negative controls and calibration experiments. The positive control samples were wells with bacterial suspension only, and the negative control samples were wells with tested materials only.

We examined the antibacterial properties of the polymerized tested materials using DCT immediately after polymerization and after aging them in PBS for one, two, seven and 14 days. During the aging process, we renewed the PBS every 24 hours. We performed each experiment at least three times.

pH measurements. We determined the pH values of the self-etching adhesive systems by placing 50 µL of nonpolymerized samples in 1.6 mL cuvettes using a pH meter probe (CyberScan 510, Eutec Instruments, Singapore). Simultaneously with the nonpolymerized samples, we placed two sets of polymerized samples in 15 mL tubes (Corning, Corning, N.Y.) and added 1 mL of double-distilled water (DDW) to each tube. We measured the pH values immediately after and 24 hours after polymerization.

Statistical analysis. We analyzed the growth curves for each well and calculated a regression line on the ascending linear portion of the curve, using the equation y = ax + b. This equation provided the value of the slope corresponding to the growth rate. Statistical analysis included two-and one-way analyses of variance (ANOVA) followed by Tukey multiple comparisons.


   RESULTS
 TOP
 ABSTRACT
 MATERIALS AND METHODS
 RESULTS
 DISCUSSION
 CONCLUSION
 REFERENCES
 
In the ADT, we found an inhibitory halo (2.0 ± 0.3 mm) only around the Clearfil Protect Bond specimens.

We performed the DCT on eight specimens of each tested material. We calculated a regression line on the linear portion of the growth curve, which represents the logarithmic growth phase. The multivariate coefficient of determination of all growth curves ranged from R2 = 0.91 to R2 = 0.99. Two-way ANOVA showed a significant difference in bacterial growth rate, both on different adhesive materials (P < .001) and at different tested times (P < .001). We observed no bacterial growth on the fresh samples of self-etching adhesives (P < .001) (data not shown).

After the materials aged for one day, we observed bacterial growth only in the Adper Prompt L-Pop sample wells, which was not significantly different from the control sample (P < .001) (Figure 2Go and Table 1Go). After aging for two days, Clearfil Protect Bond sample wells showed no bacterial growth. We observed bacterial growth in the AdheSe, Adper Prompt L-Pop and Xeno III samples, with no significant difference from the control in the Adper Prompt L-Pop and Xeno III samples (P < .001) (Figure 3Go and Table 1Go). After aging for seven days, the Clearfil Protect Bond samples still showed antibacterial properties (P < .001); the other tested materials did not differ from the control (Table 1Go). After aging for 14 days, none of the tested self-etching adhesive materials exhibited any antibacterial properties (Table 1Go).


Figure 2
View larger version (44K):
[in this window]
[in a new window]

 
Figure 2. Bacterial outgrowth (measured by changes in optical density [OD]) on the surface of self-etching adhesive materials after aging for one day. Each point is the average OD measured simultaneously in eight wells. AdheSe is manufactured by Ivoclar Vivadent, Schaan, Liechtenstein. Adper Prompt L-Pop is manufactured by 3M ESPE, Seefeld, Germany. Clearfil Protect Bond is manufactured by Kuraray, Kurashiki, Okayama, Japan. Xeno III is manufactured by Dentsply, Konstanz, Germany.

 

View this table:
[in this window]
[in a new window]

 
TABLE 1 Bacterial growth rate after direct contact with tested materials.

 

Figure 3
View larger version (49K):
[in this window]
[in a new window]

 
Figure 3. Bacterial outgrowth (measured by changes in optical density [OD]) on the surface of self-etching adhesive materials after aging for two days. Each point is the average OD measured simultaneously in eight wells. AdheSe is manufactured by Ivoclar Vivadent, Schaan, Liechtenstein. Adper Prompt L-Pop is manufactured by 3M ESPE, Seefeld, Germany. Clearfil Protect Bond is manufactured by Kuraray, Kurashiki, Okayama, Japan. Xeno III is manufactured by Dentsply, Konstanz, Germany.

 
The pH value measurements of self-etching adhesive materials before, immediately after and 24 hours after polymerization are shown in Table 2Go.


View this table:
[in this window]
[in a new window]

 
TABLE 2 pH measurements of tested self-etching adhesive materials.

 

   DISCUSSION
 TOP
 ABSTRACT
 MATERIALS AND METHODS
 RESULTS
 DISCUSSION
 CONCLUSION
 REFERENCES
 
The ADT is used as the standard assay to measure antibacterial properties of materials, despite its limitations23 (that is, it measures only components that are water-soluble). In our study, we also used the DCT, which measures the effect of direct and close contact between the microorganism and the tested materials. Antibacterial properties are assessed regardless of their solubility and the diffusiveness of components into the surrounding area.1822,24

The results from the ADT showed that only Clearfil Protect Bond exhibited a large inhibition halo, suggesting that soluble antibacterial components were released into the surrounding environment. Under DCT conditions, all of the tested adhesives had an immediate bactericidal effect on S. mutans. However, all of the materials lost their antibacterial properties within 14 days: Adper Prompt L-Pop after 24 hours, AdheSe and Xeno III within 48 hours and Clearfil Protect Bond after 14 days. It is reasonable to assume that their antibacterial components decomposed at varying rates into the surrounding aging liquid. The prolonged antibacterial effect of Clearfil Protect Bond is related to the antibacterial properties of the MDPB molecules,6,25 which become immobilized after adhesive photopolymerization.6,25,26 Our findings both in ADT and DCT, however, did not support this assumption. We hypothesize that not all MDPB molecules copolymerize, and those that do not are able to leach and manifest their antimicrobial properties. Once all the MDPB molecules that did not copolymerize are leached out, the antimicrobial effect disappears.

The advantage of the obtained prolonged antibacterial effect due to possible toxicity of the released antibacterial component on human tissues is questionable.25 It also is questionable whether this short-term antibacterial period (14 days) has a significant clinical advantage over the 24-hour antibacterial activity exhibited by other bonding systems.

The results we obtained in this study do not support a previously stated hypothesis that the antibacterial effect of self-etching adhesive systems is related to the acidic nature of nonpolymerized materials.6,27,28 Our results are in agreement with those of Imazato and colleagues29 who suggested that the benefit of a low pH environment exhibited by dentin bonding systems should be considered as "limited."


   CONCLUSION
 TOP
 ABSTRACT
 MATERIALS AND METHODS
 RESULTS
 DISCUSSION
 CONCLUSION
 REFERENCES
 
The application of self-etching adhesive materials could contribute toward completely eliminating bacteria or minimizing it during tooth preparation. Since none of the self-etching adhesive systems tested had long-lasting antibacterial properties, they did not provide a solution to the main cause for secondary caries: bacterial invasion owing to microleakage.


   FOOTNOTES
 

Dr. Feuerstein is a lecturer, Department of Prosthodontics, Faculty of Dental Medicine, Hebrew University, Jerusalem.


Dr. Matalon is a lecturer, Department of Oral Rehabilitation, The Maurice and Gabriela Goldschleger School of Dental Medicine, Tel Aviv University, Tel Aviv, Israel 69978, e-mail "matalons@post. tau.ac.il". Address reprint requests to Dr. Matalon.


Dr. Slutzky is a clinical instructor, Department of Prosthodontics, Faculty of Dental Medicine, Hebrew University, Jerusalem.


Dr. Weiss is a professor, Department of Prosthodontics, Faculty of Dental Medicine, Hebrew University, Jerusalem.


This research was conducted at the Ronald E. Goldstein Center for Esthetic Dentistry and Dental Material Research, Hebrew University-Hadassah School of Dental Medicine, Jerusalem. The authors thank Ms. Rita Lazar for editorial assistance.


   REFERENCES
 TOP
 ABSTRACT
 MATERIALS AND METHODS
 RESULTS
 DISCUSSION
 CONCLUSION
 REFERENCES
 

  1. Toledano M, Osorio R, Ceballos L, et al. Microtensile bond strength of several adhesive systems to different dentin depths. Am J Dent 2003;16(5):292–8.[Medline]

  2. van Dijken JW. Durability of three simplified adhesive systems in Class V non-carious cervical dentin lesions. Am J Dent 2004;17(1): 27–32.[Medline]

  3. Tay FR, Carvalho R, Sano H, Pashley DH. Effect of smear layers on the bonding of self-etching primer to dentin. J Adhes Dent 2000;2(2):99–116.[Medline]

  4. Kidd EA. Diagnosis of secondary caries. J Dent Educ 2001;65(10): 997–1000.[Abstract]

  5. Brunthaler A, Konig F, Lucas T, Sperr W, Schedle A. Longevity of direct resin composite restorations in posterior teeth. Clin Oral Investig 2003;7(2):63–70.[Medline]

  6. Imazato S, Ehara A, Torii M, Ebisu S. Antibacterial activity of dentine primer containing MDPB after curing. J Dent 1998;26(3):267–71.[Medline]

  7. Ohmori K, Maeda N, Kohno A. Evaluation of antibacterial activity of three dentin primers using an in vitro tooth model. Oper Dent 1999;24(5):279–85.[Medline]

  8. Emilson CG, Bergenholtz G. Antibacterial activity of dentinal bonding agents. Quintessence Int 1993;24(7):511–5.[Medline]

  9. Palenik CJ, Setcos JC. Antimicrobial abilities of various dentine bonding agents and restorative materials. J Dent 1996;24(4):289–95.[Medline]

  10. Prati C, Fava F, Di Gioia D, Selighini M, Pashley DH. Antibacterial effectiveness of dentin bonding systems. Dent Mater 1993;9(6): 338–43.[Medline]

  11. Meiers JC, Miller GA. Antibacterial activity of dentin bonding systems, resin-modified glass ionomers and polyacid-modified composite resins. Oper Dent 1996;21(6):257–64.[Medline]

  12. Scherer W, Lippman N, Kaim J, LoPresti J. Antimicrobial properties of VCL liners. J Esthet Dent 1990;2(2):31–2.[Medline]

  13. Imazato S, Kinomoto Y, Tarumi H, Torii M, Russell RR, McCabe JF. Incorporation of antibacterial monomer MDPB in dentin primer. J Dent Res 1997;76(3):768–72.[Abstract/Free Full Text]

  14. Eli I, Cooper Y, Ben-Amar A, Weiss E. Antibacterial activity of three dental liners. J Prosthodont 1995;4(3):178–82.[Medline]

  15. Herrera M, Carrion P, Baca P, Liebana J, Castillo A. In vitro antibacterial activity of glass-ionomer cements. Microbios 2001; 104(409):141–8.[Medline]

  16. Herrera M, Castillo A, Baca P, Carrlon P. Antibacterial activity of glass-ionomer restorative exposed to cavity-producing microorganisms. Oper Dent 1999;24(5):286–91.[Medline]

  17. Herrera M, Castillo A, Bravo M, Liebana J, Carrion P. Antibacterial activity of resin adhesives, glass ionomer and resin-modified glass ionomer cements and compomer in contact with dentin caries samples. Oper Dent 2000;25(4):265–9.[Medline]

  18. Matalon S, Slutzky H, Mazor Y, Weiss EI. Surface antibacterial properties of fissure sealants. Pediatr Dent 2003;25(1):43–8.[Medline]

  19. Fuss Z, Weiss EI, Shalhav M. Antibacterial activity of calcium hydroxide-containing endodontic sealers on Enterococcus faecalis in vitro. Int Endod J 1997;30(6):397–402.[Medline]

  20. Weiss EI, Shalhav M, Fuss Z. Assessment of antibacterial activity of endodontic sealers by a direct contact test. Endod Dent Traumatol 1996;12(4):179–84.[Medline]

  21. Matalon S, Slutzky H, Weiss EI. Surface antibacterial properties of packable resin composites: part I. Quintessence Int 2004;35(3): 189–93.[Medline]

  22. Slutzky H, Matalon S, Weiss EI. Antibacterial surface properties of polymerized single-bottle bonding agents: part II. Quintessence Int 2004;35(4):275–9.[Medline]

  23. Tobias RS. Antibacterial properties of dental restorative materials: a review. Int Endod J 1988;21(2):155–60.[Medline]

  24. Lewinstein I, Matalon S, Slutzkey S, Weiss EI. Antibacterial properties of aged dental cements evaluated by direct-contact and agar diffusion tests. J Prosthet Dent 2005;93(4):364–71.[Medline]

  25. Imazato S, Torii Y, Takatsuka T, Inoue K, Ebi N, Ebisu S. Bactericidal effect of dentin primer containing antibacterial monomer methacryloyloxydodecylpyridinium bromide (MDPB) against bacteria in human carious dentin. J Oral Rehabil 2001;28(4):314–9.[Medline]

  26. Imazato S, Ebi N, Tarumi H, Russel RR, Kaneko T, Ebisu S. Bactericidal activity and cytotoxicity of antibacterial monomer MDPB. Bio-materials 1999;20(9):899–903.[Medline]

  27. Imazato S, Imai T, Ebisu S. Antibacterial activity of proprietary self-etching primers. Am J Dent 1998;11(3):106–08.[Medline]

  28. Ohmori K, Maeda N, Kohno A. Evaluation of antibacterial activity of three dentin primers using an in vitro tooth model. Oper Dent 1999;24(5):279–85.[Medline]

  29. Imazato S. Antibacterial properties of resin composites and dentin bonding systems. Dent Mater 2003;19(6):449–57.[Medline]




This article has been cited by other articles:


Home page
JDRHome page
F. Li, Z.G. Chai, M.N. Sun, F. Wang, S. Ma, L. Zhang, M. Fang, and J.H. Chen
Anti-biofilm Effect of Dental Adhesive with Cationic Monomer
Journal of Dental Research, April 1, 2009; 88(4): 372 - 376.
[Abstract] [Full Text] [PDF]


This Article
Right arrow Abstract Freely available
Right arrow Full Text (PDF)
Right arrow Alert me when this article is cited
Right arrow Alert me if a correction is posted
Services
Right arrow Similar articles in this journal
Right arrow Similar articles in PubMed
Right arrow Alert me to new issues of the journal
Right arrow Download to citation manager
Right arrow reprints & permissions
Citing Articles
Right arrow Citing Articles via HighWire
Right arrow Citing Articles via Google Scholar
Google Scholar
Right arrow Articles by Feuerstein, O.
Right arrow Articles by Weiss, E. I.
Right arrow Search for Related Content
PubMed
Right arrow PubMed Citation
Right arrow Articles by Feuerstein, O.
Right arrow Articles by Weiss, E. I.
Related Collections
Right arrow Infection Control


HOME HELP FEEDBACK SUBSCRIPTIONS ARCHIVE SEARCH TABLE OF CONTENTS